Repository LOGO
    • Login
    View Item 
    •   Intellectual Repository at Rajamangala University of Technology Phra Nakhon
    • Office of the President (สำนักงานอธิการบดี)
    • International Affairs Division
    • The First RMUTP International Conference
    • View Item
    •   Intellectual Repository at Rajamangala University of Technology Phra Nakhon
    • Office of the President (สำนักงานอธิการบดี)
    • International Affairs Division
    • The First RMUTP International Conference
    • View Item
    JavaScript is disabled for your browser. Some features of this site may not work without it.

    Browse

    All of DSpaceCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CollectionBy Issue DateAuthorsTitlesSubjects

    My Account

    Login

    Silk Degumming with Dried Latex of Carica Papaya Linn

    Thumbnail
    View/Open
    Silk Degumming with Dried Latex of Carica Papaya Linn.pdf (328.3Kb)
    Date
    2009-07-13
    Author
    Sasithorn, Nongnut
    Luepong, Kanchana
    Metadata
    Show full item record
    Abstract
    Degumming process is a fundamental finishing process for silk yarn and silk fabric. The main objective is scouring the substrate such as silk gum (sericin), wax and some impurities from silk fiber. The principle of degumming process is breaking the peptide linkage of amino acid in sericin structure into a small molecule, which is soluble in water. The hydrolysis reaction performed by acid and alkaline, but they have a big problem on the surface area of silk. Proteolytic enzyme be used to solve this problem but it has some disvantages such as it was using a specific condition and expensive. For this reason, this research chooses papain enzyme form dried latex of Carica payapa Linn. to degum the raw silk. The efficiency of degumming process was evaluated by determination of tensile strength and staining test with direct dyes (C.I. Direct Red 80). The result was revealed; the appropriate conditions for silk degumming with dried Carica payapa Linn.’s latex be recommended as follows: the amount of dried latex solution of 4 % owf at 75 degree Celsius for 30 minutes, in this condition was not harm to strength and fiber surface. The degummed fibers still had lustrous, soft and smooth surface.
    URI
    http://repository.rmutp.ac.th/handle/123456789/301
    Collections
    • The First RMUTP International Conference [18]

    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV
     

     


    DSpace software copyright © 2002-2015  DuraSpace
    Contact Us | Send Feedback
    Theme by 
    @mire NV